Select Language
Inquiry Basket ( 0 )
Company Details
  • Luoyang Golden Egret Geotools Co., Ltd

  •  [Henan,China]
  • Business Type:Manufacturer
  • Main Markets: Worldwide , Americas , Asia , East Europe , Europe , Middle East , North Europe , Oceania , Other Markets , West Europe
  • Exporter:41% - 50%
  • Certs:ISO14001, ISO9001, MSDS, Test Report
Luoyang Golden Egret Geotools Co., Ltd

Luoyang Golden Egret Geotools Co., Ltd

Home > News > Development status of preparation technology of nickel-based superalloy powder

News

Development status of preparation technology of nickel-based superalloy powder

2024-09-15

Vacuum induction melting gas atomization (VIGA process)
4da91f2466ec0f4ec283ba6b0dfb360
Vacuum induction melting gas atomization method means that in vacuum environment, the coil induction heating principle is used to melt the charge, after reaching a certain temperature, the melting chamber and atomization chamber are filled with atomizing gas, and then the molten steel is poured into the tunic, and the metal liquid flow is formed through the nozzle into the atomization chamber [18], and then the high-pressure inert gas is used as the atomizing medium to break the continuous metal liquid flow. It quickly solidifies into fine particles, that is, metal powder. FIG. 1 shows the schematic diagram of aerosol vaporization principle.
 
Figure 2 shows the powder produced by vacuum induction melting gas atomization process. From the surface morphology, it can be seen that the particle size of the powder obtained by gas atomization method is dispersed, generally about a few microns to more than 100 microns, and the sphericity is preferred, but there are satellite powder and adhesion powder.
e89fd5152fc43d6df66499862da809f
There are a lot of non-spherical powder, satellite powder, adhesion powder, hollow powder, particle size dispersion and more non-metallic impurities in the powder prepared by aerosol method. At present, the mainstream powder making method in Europe and the United States is aerosol powder making, among which GE company, ALD and other companies are in a leading position in the field of aerosol powder making equipment. There are also many companies that manufacture vacuum induction melting gas atomization equipment in China, such as: Shenyang Vacuum Technology Institute Hunan Jiutai, Hunan Tianji Wisdom and so on. Companies that use VIGA to produce metal powder materials abroad include Sandvik, Hegners, Oerekon, LPW, Tycona, TLS and so on. There are also many excellent metal powder suppliers in China, such as Beijing Steel Research Institute Gaona, Beijing AVIC Met, Jiangsu Willari, Wuxi fly Kang and so on. At present, the use of vacuum induction melting gas atomization powder, in addition to nickel based superalloy powder, other metal powder materials are: stainless steel 316L, 174PH; Cobalt base alloys CoCrMo, CoCrW, CoCrMoW; Titanium and titanium alloys TC4, TC11TA15, TiAl4822, Ti2AlNb; Nickel-based alloys FGH95, FGH96, FGH97, GH4169, rare metals, etc.
 
Share to:  
Previous: Nickel based superalloy powder preparation technology - electric separation technology Next: 【 Exhibition Topic 】 Luoyang Golden Egret will appear at the 2024 MINExpo
Communicate with Supplier?Supplier
Fiona Cui Ms. Fiona Cui
What can I do for you?
Contact Supplier